    tube bending

    how do u determin how much tube u need before makin a bend

  2. #2
    Senior Member RACING JUNKIE
    Join Date
    Sep 2007
    Posts
    4,143
    You must know the radius of the bend you are going to make.Then you figure the stretch factor of the tube.This will tell you how much tube is required just to go from tangent to tangent on the bend. Then you add in the length of the straights. I bend tubes for a living. I have the formula for figuring stretch factor at work. I am at home now.If you want it I can post it up later tonight on my lunch break.

    tangent = where the straight stops and the bend starts


Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •  
Copyright © 2005-2016 RacingJunk.com All Rights Reserved.

Designated trademarks and brands are the property of their respective owners. Use of this Web site constitutes acceptance of the RacingJunk.com
Terms of Use, Classifieds Disclaimer, Privacy Policy, and Cookie Policy